AASHTO T 363
$47.00
Standard Method of Test for Evaluating Stress Development and Cracking Potential due to Restrained Volume Change Using a Dual Ring Test
Published by | Publication Date | Number of Pages |
AASHTO | 2017 | 8 |
Description
AASHTO T 363 – Standard Method of Test for Evaluating Stress Development and Cracking Potential due to Restrained Volume Change Using a Dual Ring Test
This test method covers the evaluation of stress development and cracking potential in concretewhen volume changes caused by shrinkage and temperature changes are restrained. The procedureis comparative for the degree of restraint of the ring and is not intended to determine the time ofinitial cracking of a concrete cast in any specific type of structure.
Product Details
- Published:
- 2017
- Number of Pages:
- 8
- File Size:
- 1 file , 1.4 MB
- Product Code(s):
- T363-17-UL, T363-17-UL, T363-17-UL
- Note:
- This product is unavailable in Ukraine, Russia, Belarus